[Discussion] Pearlescent OPP, surface printing ink: small trailing streaks keep appearing when printing large spot-color areas, at both high and low viscosity—what should we do?
A flexible packaging company: When printing large spot-color areas on a surface-printed product, small trailing streaks keep appearing, at both high and low viscosity. After wiping with a chopstick, they reappear after a while. Is it because the machine speed is too slow, the ink particles are too coarse, or some other reason? Pearlescent OPP, surface printing ink.
Shenzhen - Packaging Bags: Try filtering the ink.
Yinteng Packaging - Yu Dingzhao: The ink probably has impurities. Try filtering it.
Shangyang Packaging - Qi: Try adding a small amount of water to the ink.
Yinteng Packaging - Yu Dingzhao: Adding water is rarely used, but those who use it are experts. I heard that at most 1.5KG of water can be added to 20KG of ink. I haven't verified it—have you tried it?
Shangyang Packaging - Qi: When ordinary PET and OPP inks produce ink lines, adding a little water during production often solves the problem. But don't add too much—too much won't work. I saw this at Zhongshan Tiancai, and the effect was really good. You can try it on a small scale.
A flexible packaging company: Can water be added to surface printing ink?
Yinteng Packaging - Yu Dingzhao: I just asked a technician. The role of adding water to ink is to eliminate static electricity in the ink and increase the slipperiness between the plate and the doctor blade.
Guangzhou Yiying Color Printing: Check whether there is any regularity. If regular, it may be the blade; if irregular, it is static electricity. Does it appear along the blade's oscillation path? First check for regularity, then consider the ink and other causes. The blade oscillates; if the back-and-forth distance is the same, that is regularity. If it is the plate, it stays fixed. If the drag marks are irregular, you can add antistatic liquid to the ink to prevent trailing.
Yantai Flexible Packaging - Wu: It should be caused by overly large ink particles. Also check whether the doctor blade is clogged. Static electricity causes burrs, not blade streaks. What is the workshop humidity?
Zhuhai Ruilong Water Ink: It should be caused by insufficient ink fineness.
Wu Xianchao: This kind of problem is generally a plate or ink issue. Ink: control the proportion of old ink used, filter the ink; control dust in the environment. Plate: when copper plating, ask the plate-making factory to grind it once; during use, if problems occur, polish the plate.
Sichuan Tianyi - Li: Polish the plate cylinder and try a smaller doctor blade angle.
Yantai Flexible Packaging - Wu: First polish the plate cylinder.
Wu Xianchao: Polishing the plate cylinder before chrome plating gives the best effect. (From the Packaging Frontier flexible packaging technology QQ group. You are welcome to join: Main group: 121451012; Group I: 64311965; Group II: 37848282; Group III: 119411638; Group IV: 116162302; Group V: 256925591. For more technical content, see the bimonthly magazine Packaging Frontier. Welcome to subscribe: Mr. Xie: 020~85626447/605, 13310896471. For more content, visit the Packaging Frontier website www.pack168.com.)
Related reading
- Shanghai Municipal Administration for Market Regulation Releases the Sixth Batch of Typical Cases in the Special Campaign on Online Catering Food Safety2026-11-04Industry NewsSource: 食品伙伴网
In order to further advance the special campaign on online catering food safety and continuously consolidate the results of governance, the Shanghai Municipal Administration for Market Regulation has adhered to a problem-oriented approach, made simultaneous efforts online and offline, strictly investigated food safety risks and hidden dangers, and cracked down on illegal and non-compliant acts such as "ghost takeaways" and false advertising, resolutely safeguarding the safety of the food on the people's plates. The sixth batch of typical cases is hereby released as follows, in the hope that the majority of online catering operators will take these cases as a warning, learn from the examples, earnestly fulfill their primary responsibility for food safety, and jointly
- What Does Packaging "Slimming Down" and "Lightening Up" Bring?2026-11-03Industry NewsSource: 中国包装网
1. Takeout packaging "slims down," letting the right packaging "carry" the right food "No more tearing plastic wrap by hand!" Since the semester began, Jiao Ke, a student at a university in Beijing, and his roommates have found that the takeout they usually order has changed dramatically in its packaging! "In the past, the plastic wrap was wound three times one way and three times the other—you'd be left doubting life itself before you got it open! Now the packaging is clean and neat; just lift the lid and enjoy the food," he said outright. For some time now, excessive packaging with "big boxes for small meals and layer upon layer added" has become excessive
- Beijing Issues New Rules on Takeout Packaging2026-11-02Industry NewsSource: 中国包装网
Buns in bags, soup noodles in sealed boxes, barbecue wrapped in aluminum foil... How can takeout packaging be both environmentally friendly and practical? Beijing has given a new answer. Recently, the Municipal Market Regulation Bureau released the local standard "Guidelines for the Use of Green Packaging by Food Delivery Merchants," which is scheduled to be officially implemented from September 1. This document, known in the industry as the takeout "slimming" standard, provides food delivery merchants with a clear operating manual, covering everything from packaging materials and usage specifications to classification methods. What is "green pack
- Nearly 70% of Non-Compliant Items Come from Seafood and Meat! Interpreting the August 2026 Notification on Imported Food Refused Entry2026-10-31Industry NewsSource: 食品伙伴网
Foodmate Network, September 2026 — The General Administration of Customs reported that in August 2026, customs authorities nationwide detected 755 batches of food that failed quality and safety items and were refused entry during supervision at the port-of-entry stage. The refused food came from 42 countries or regions and involved 22 product categories, mainly aquatic products and their products, meat and meat products, sugar confectionery and chocolate, cocoa and its products, etc. The main non-compliance item was illegal use of sodium metabisulfite
Contact us for a quote
For samples, pricing or technical support, call us or leave a message and we will reply shortly.
+86 15916881866 Contact us